Molds & Tooling 8 visualizaciones

GPPS Product Sink Marks

Fenómeno del problema
Depressions appear on the back of thick walls and rib positions.
Análisis de la causa
Shrinkage at uneven wall thickness is not compensated; insufficient holding pressure or early gate freezing aggravates sink marks.; during on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience
Solución
①Increase holding pressure and time; ②core out thick areas; ③enlarge gates; ④optimize wall thickness design.; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Conclusión clave
GPPS sink marks follow the feeding mechanism; structural uniformity is the fundamental solution.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future
PS;GPPS;sink mark;holding pressure;wall thickness;coring out