PSU Extrusion Molding Defects
Fenómeno del problema
PSU extruded sheets and pipes show surface roughness and internal stress; the extrusion process window is narrow; scrap rate is high.
Análisis de la causa
PSU extrusion barrel temperature gradually rises from 320 to 400°C; low rotation speed reduces shear heat; die temperature 150~200°C for shaping; mismatched process parameters cause frequent defects.
Solución
①Barrel temperature controlled in stages from 320 to 400°C; ②Low screw rotation speed; ③Die temperature 150~200°C; ④Dedicated high-torque equipment configuration.
Conclusión clave
PSU extrusion has clear temperature and rotation speed specifications; high-viscosity materials require dedicated equipment; the process window is set according to material characteristics.; After confirming effectiveness, solidify the parameters and practices into the work instructions to prevent recurrence