Injection Molding 3 visualizaciones

PVC Injection Flow Marks

Fenómeno del problema
Dark flow marks appear on product surface, uneven gloss, poor appearance.
Análisis de la causa
Uneven plasticization, large melt temperature gradient; PVC melt has high elasticity, unstable flow shows marks on the surface; uneven melt temperature or poor plasticization makes local melt state inconsistent, forming visible flow marks.
Solución
①Improve plasticization uniformity; ②Stabilize the melt temperature curve, avoid quality drift caused by temperature fluctuation; ③Optimize the injection speed curve; ④Enlarge gates and runners; ⑤Increase mold temperature to improve flow front contact.
Conclusión clave
PVC flow marks = a 'plasticization uniformity' problem: uneven plasticization is the root; PVC melt has high elasticity, any slight flow instability leaves marks on the surface — uniformity of plasticization and temperature control is fundamental.
PVC; '2079851475616104452; flow mark; plasticization; melt temperature