Injection Molding
2 visualizações
PVC Injection Flow Marks
Fenómeno do problema
Dark flow marks appear on product surface, uneven gloss, poor appearance.
Análise das causas
Uneven plasticization, large melt temperature gradient; PVC melt has high elasticity, unstable flow shows marks on the surface; uneven melt temperature or poor plasticization makes local melt state inconsistent, forming visible flow marks.
Solução
①Improve plasticization uniformity; ②Stabilize the melt temperature curve, avoid quality drift caused by temperature fluctuation; ③Optimize the injection speed curve; ④Enlarge gates and runners; ⑤Increase mold temperature to improve flow front contact.
Conclusão principal
PVC flow marks = a 'plasticization uniformity' problem: uneven plasticization is the root; PVC melt has high elasticity, any slight flow instability leaves marks on the surface — uniformity of plasticization and temperature control is fundamental.
Isto foi útil?
0 pessoas acharam isto útil
Obrigado pelo seu comentário!