Extrusion & Post
9 visualizaciones
PVC Profile Uneven Cooling Deformation
Fenómeno del problema
Profile bends after exiting calibration die, poor straightness.
Análisis de la causa
Uneven cooling, calibration die wear, haul-off skew; inconsistent cooling of profile parts produces bending stress; during on-site troubleshooting, verify item by item according to this mechanism, avoid blindly adjusting the machine based solely on experience.
Solución
①Evenly arrange cooling water channels to ensure consistent cooling of all parts; ②Overhaul calibration die wear and water channels; ③Correct haul-off straightness to ensure profile not bent; ④Optimize wall thickness distribution to reduce wall thickness sudden changes; ⑤Stabilize extrusion output and pressure.
Conclusión clave
PVC profile bending = 'cooling and haul-off straightness': uniform cooling and straight haul-off are the two elements; calibration die condition directly determines profile straightness; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.
¿Le ha resultado útil?
0 personas encontraron esto útil