Processing Machinery
7 visualizaciones
PVC Screw Temperature
Fenómeno del problema
After PVC screw wear, product degradation points increase
Análisis de la causa
Worn screw clearance backflow makes material residence time uneven, local overheating degradation; during on-site troubleshooting, verify item by item according to this mechanism, avoid blindly adjusting the machine based solely on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Solución
Screw wear regularly detected; replace when wear exceeds standard; select PVC-dedicated low-shear screw; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Conclusión clave
Screw condition is part of PVC residence control; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems later
¿Le ha resultado útil?
0 personas encontraron esto útil
¡Gracias por sus comentarios!