Processing Machinery
6 visualizações
PVC Screw Temperature
Fenómeno do problema
After PVC screw wear, product degradation points increase
Análise das causas
Worn screw clearance backflow makes material residence time uneven, local overheating degradation; during on-site troubleshooting, verify item by item according to this mechanism, avoid blindly adjusting the machine based solely on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Solução
Screw wear regularly detected; replace when wear exceeds standard; select PVC-dedicated low-shear screw; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Conclusão principal
Screw condition is part of PVC residence control; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems later
Isto foi útil?
0 pessoas acharam isto útil
Obrigado pelo seu comentário!