Extrusion & Post 9 visualizaciones

TPU product paint peeling

Fenómeno del problema
Poor paint film adhesion after coating.
Análisis de la causa
Surface release agent or exudates hinder adhesion; TPU elastic deformation also cracks the paint film; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
Solución
①clean the surface before coating; ②select elastic paint systems; ③control the use of release agent; ④do adhesion testing; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Conclusión clave
TPU coating requires a clean surface and matching paint type; elastic substrates need flexible coatings; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
TPU;spraying;paint peeling;adhesion;elastic paint;cleaning