Extrusion & Post 14 visualizaciones

Severe screw wear of EAA extruder

Fenómeno del problema
After 200h of EAA extrusion, the wear of the screw and barrel reaches 0.5mm
Análisis de la causa
The filler causes large wear on the screw; the screw material hardness is insufficient, not nitrided; high processing temperature causes EAA to adhere to the screw and aggravate wear
Solución
1) Use nitrided screws or bimetallic screws of SK-2 alloy; 2) Lower the processing temperature to reduce adhesive wear; 3) Treat the filler with a coupling agent to reduce friction; 4) Regularly check the wear, replace in time when >0.3mm
Conclusión clave
Screw wear is caused by filler friction and adhesion; wear-resistant screws and temperature control are the key
EAA extrusion screw wear nitrided screw filler friction bimetallic screw