EAA internal inclusions
Fenómeno del problema
Inclusions of 0.1-0.5mm inside EAA products affecting appearance
Análisis de la causa
Impurity particles in the raw material; dust contamination from the production environment; foreign matter mixed into recycled material
Solución
1) Filter raw material through a 120-mesh screen to remove impurities; 2) Keep the production environment clean and control dust; 3) Strictly sort recycled material to remove foreign matter
Conclusión clave
Inclusions are caused by raw material and environmental contamination; filtration and environmental control are key