Fenómeno del problema
EEA products gradually yellow on the surface after 1 week of storage, color difference ΔE>3
Análisis de la causa
Incomplete antioxidant system, thermal oxidative degradation producing yellow products; ultraviolet irradiation accelerating photo-oxidation; residual transition metal catalysts catalyzing oxidation
Solución
1) Improve the antioxidant system 1010(0.1)+168(0.1)+DSTDP(0.2)wt%; 2) Add UV absorber 0.2-0.5wt%; 3) Add metal deactivator 0.05wt%; 4) Select low-residue raw material grade
Conclusión clave
Yellowing is caused by thermal and photo oxidation and metal catalysis; improving the antioxidant system and UV absorber is the key