EEA performance degradation with repeated processing
Fenómeno del problema
EEA after 3-4 times of recycling and reprocessing shows tensile strength decline of 25-30%
Análisis de la causa
Molecular chains break and degrade under repeated high temperature and shear; antioxidant exhausted in multiple processing; cumulative effect of thermo-mechanical degradation
Solución
1) Recycled material proportion not exceeding 20-30%; 2) Supplement 0.1-0.2wt% antioxidant at each re-extrusion; 3) Reduce processing temperature by 5-10°C; 4) Reduce screw speed to reduce shear
Conclusión clave
Performance degradation from multiple processing is caused by thermo-mechanical degradation; limiting recycled material and supplementing antioxidant are the key