Processing Machinery 8 visualizaciones

EEA Internal Unmelted Particles

Fenómeno del problema
Unmelted transparent or translucent particles appear inside EEA products
Análisis de la causa
Insufficient screw plasticizing capacity, temperature low; feeding amount too large, exceeding plasticizing capacity; EEA melting temperature high
Solución
1) Increase processing temperature to ensure full melting; 2) Reduce feeding amount to match plasticizing capacity; 3) Increase screw mixing section
Conclusión clave
Unmelted particles are caused by insufficient plasticization; increasing temperature and reducing feeding are key
EEA unmelted particles plasticizing capacity processing temperature screw mixing

¿Le ha resultado útil?

0 personas encontraron esto útil

ChemAI