EEA Internal Unmelted Particles
Fenómeno do problema
Unmelted transparent or translucent particles appear inside EEA products
Análise das causas
Insufficient screw plasticizing capacity, temperature low; feeding amount too large, exceeding plasticizing capacity; EEA melting temperature high
Solução
1) Increase processing temperature to ensure full melting; 2) Reduce feeding amount to match plasticizing capacity; 3) Increase screw mixing section
Conclusão principal
Unmelted particles are caused by insufficient plasticization; increasing temperature and reducing feeding are key