Extrusion & Post 15 visualizaciones

EMA Extruded Film Wrinkling During Winding

Fenómeno del problema
Transverse wrinkles and longitudinal creases appear after winding of EMA extruded film
Análisis de la causa
Film tension uneven, fluctuating ±20%; film thickness uneven, causing inconsistent stretching of each section; shrinkage rates differ in each direction after cooling
Solución
1) Automatic tension control system to stabilize winding tension; 2) Improve film thickness uniformity to ±5%; 3) Adjust guide roller parallelism <0.05mm/m; 4) Fully cool the film to <30°C before winding
Conclusión clave
Film wrinkling is caused by tension fluctuation and uneven thickness; automatic tension control and uniformization are key