EMA surface stress whitening
Fenómeno del problema
Stress whitening appears on the surface of stressed areas of EMA products, affecting appearance and strength
Análisis de la causa
Under local stress, EMA molecular orientation causes refractive index differences and whitening; areas of internal stress concentration in the product
Solución
1) Reduce injection speed to reduce orientation stress; 2) Annealing treatment at 80°C/2h to release stress; 3) Product design avoids stress-concentrating sharp corners
Conclusión clave
Stress whitening is caused by orientation and internal stress; reducing orientation and annealing are key