Material Analysis 15 visualizaciones

Dimensional change of EVA products during long-term storage

Fenómeno del problema
After 3 months of storage, EVA product dimensions change ±2-3%, exceeding the ±0.5% requirement
Análisis de la causa
EVA physical aging relaxation causes continuous dimensional change; secondary crystallization slowly changes density and dimensions; low molecular substances slowly migrate changing local density
Solución
1) Annealing treatment at 80°C/4h before shipment to stabilize dimensions; 2) Select high molecular weight grade to reduce low molecular substances; 3) Slight crosslinking to reduce molecular chain mobility and inhibit aging; 4) Control storage environment temperature at 23±2°C to reduce temperature change influence
Conclusión clave
Dimensional change is caused by physical aging; annealing treatment and slight crosslinking are measures to stabilize dimensions
EVA dimensional stability physical aging annealing secondary crystallization slight crosslinking