Material Analysis
14 visualizações
Dimensional change of EVA products during long-term storage
Fenómeno do problema
After 3 months of storage, EVA product dimensions change ±2-3%, exceeding the ±0.5% requirement
Análise das causas
EVA physical aging relaxation causes continuous dimensional change; secondary crystallization slowly changes density and dimensions; low molecular substances slowly migrate changing local density
Solução
1) Annealing treatment at 80°C/4h before shipment to stabilize dimensions; 2) Select high molecular weight grade to reduce low molecular substances; 3) Slight crosslinking to reduce molecular chain mobility and inhibit aging; 4) Control storage environment temperature at 23±2°C to reduce temperature change influence
Conclusão principal
Dimensional change is caused by physical aging; annealing treatment and slight crosslinking are measures to stabilize dimensions
Isto foi útil?
0 pessoas acharam isto útil
Obrigado pelo seu comentário!