Injection Molding
2 visualizaciones
EVA surface color difference is obvious
Fenómeno del problema
EVA products have inconsistent color depth in different parts, color difference ΔE>5
Análisis de la causa
Uneven dispersion of color masterbatch; pigment orientation during injection causing uneven color distribution; barrel temperature fluctuation causing color change
Solución
1) Color masterbatch masterbatch method to ensure uniform dispersion; 2) Reduce injection speed to reduce pigment orientation; 3) Stabilize barrel temperature ±2°C
Conclusión clave
Color difference is caused by uneven dispersion and orientation; masterbatch method and stable processing are key