Injection Molding 1 visualizações

EVA surface color difference is obvious

Fenómeno do problema
EVA products have inconsistent color depth in different parts, color difference ΔE>5
Análise das causas
Uneven dispersion of color masterbatch; pigment orientation during injection causing uneven color distribution; barrel temperature fluctuation causing color change
Solução
1) Color masterbatch masterbatch method to ensure uniform dispersion; 2) Reduce injection speed to reduce pigment orientation; 3) Stabilize barrel temperature ±2°C
Conclusão principal
Color difference is caused by uneven dispersion and orientation; masterbatch method and stable processing are key
EVA color difference color masterbatch dispersion pigment orientation temperature stability