Processing Machinery
8 visualizaciones
Difficult EVOH Purging
Fenómeno del problema
EVOH purging takes 2-3h, time-consuming and affecting changeover efficiency
Análisis de la causa
EVOH has strong adhesion forming a firm adhesive layer on screw and barrel; EVOH has poor thermal stability, becoming sticky at high temperature and harder to remove
Solución
1) Before purging, flush with high-viscosity PE to carry away EVOH residue; 2) Reduce purging temperature below EVOH softening point to reduce adhesion; 3) Use dedicated purging compound
Conclusión clave
Purging difficulty is caused by EVOH's strong adhesion; PE flushing and temperature reduction are key
¿Le ha resultado útil?
0 personas encontraron esto útil
¡Gracias por sus comentarios!