Molds & Tooling
8 visualizaciones
Poor surface gloss of PU
Fenómeno del problema
PU product surface gloss <60%, below the 80% requirement, dull appearance
Análisis de la causa
Rough mold surface Ra>0.4μm; high PU crystallinity, surface microcrystals scatter light; improper cooling rate
Solución
1) Polish mold to Ra<0.1μm mirror finish; 2) Increase mold temperature to delay crystallization and reduce scattering; 3) Add nucleating agent to control crystal size
Conclusión clave
Poor gloss is caused by mold roughness and crystallization scattering; polishing mold and controlling crystallization are key