Extrusion & Post
14 visualizaciones
Excessive heat shrinkage of PVA film
Fenómeno del problema
PVA film heat shrinkage at 80°C >12%, exceeding the 5% dimensional stability requirement
Análisis de la causa
PVA extrusion orientation released after heating, causing large shrinkage; PVA thermal expansion coefficient large; film cooling froze a large amount of orientation stress
Solución
1) Reduce extrusion draw ratio to reduce orientation freezing; 2) Anneal film at 60-80°C to release orientation stress; 3) Add 5-10wt% rigid resin to reduce heat shrinkage; 4) Biaxial stretching process to balance orientation
Conclusión clave
Film heat shrinkage is caused by orientation freezing; reducing draw ratio and annealing treatment are key
¿Le ha resultado útil?
0 personas encontraron esto útil