Molding Process
4 visualizaciones
Poor PVA antistatic effect
Fenómeno del problema
PVA product surface resistance >10¹²Ω, severe static
Análisis de la causa
Antistatic agent addition insufficient <0.1wt%; antistatic agent migration rate slow, not reaching the surface
Solución
1) Increase antistatic agent to 0.3-0.5wt%; 2) Select an antistatic agent with fast migration rate; 3) Surface coating with antistatic liquid for immediate effect
Conclusión clave
Poor antistatic effect is caused by insufficient addition; increasing the antistatic agent is the key
¿Le ha resultado útil?
0 personas encontraron esto útil