Insufficient Flatness of CMC
Fenómeno del problema
Flatness of CMC flat products >0.5mm/100mm, warped
Análisis de la causa
CMC shrinkage is large and different in each direction; mold cooling is uneven; residual stress release causes continuous warpage
Solución
1)Uniform mold temperature to reduce temperature difference; 2)Increase holding pressure to reduce shrinkage differences; 3)Annealing to release residual stress
Conclusión clave
Insufficient flatness is caused by shrinkage differences and stress; uniform cooling and annealing are the key