Injection Molding 7 visualizaciones

DSTDP and color masterbatch mixing uneven color

Fenómeno del problema
DSTDP/color masterbatch injection molded products show color streaks and regions of uneven color depth
Análisis de la causa
Color masterbatch carrier resin incompatible with DSTDP; poor color masterbatch dispersion, pigment agglomeration; unstable melt flow during '2079851475616104452 causing pigment orientation
Solución
1) Select DSTDP or same-type carrier color masterbatch to ensure compatibility; 2) twin-screw extrusion pelletizing pre-dispersion; 3) appropriately extend mixing time to ensure pigment dispersion; 4) reduce injection speed to reduce pigment orientation
Conclusión clave
Color masterbatch carrier matching and sufficient dispersion are the key to color uniformity
DSTDP coloringcolor masterbatchcarrier compatibilitypigment dispersioncolor streaks

¿Le ha resultado útil?

0 personas encontraron esto útil