Menu
Materials Machinery
Insights
Articles Videos Problem & Solution
About
About Chembull Media Partners
Contact Us
Language
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
Back to Problem & Solution
Injection Molding 1 views

DSTDP and color masterbatch mixing uneven color

Problem Phenomenon
DSTDP/color masterbatch injection molded products show color streaks and regions of uneven color depth
Cause Analysis
Color masterbatch carrier resin incompatible with DSTDP; poor color masterbatch dispersion, pigment agglomeration; unstable melt flow during '2079851475616104452 causing pigment orientation
Solution
1) Select DSTDP or same-type carrier color masterbatch to ensure compatibility; 2) twin-screw extrusion pelletizing pre-dispersion; 3) appropriately extend mixing time to ensure pigment dispersion; 4) reduce injection speed to reduce pigment orientation
Key Takeaway
Color masterbatch carrier matching and sufficient dispersion are the key to color uniformity
DSTDP coloringcolor masterbatchcarrier compatibilitypigment dispersioncolor streaks

Was this helpful?

0 people found this helpful

ChemAI