DSTDP stress cracking
Fenómeno del problema
DSTDP product cracks under stress + chemical action in <100h
Análisis de la causa
Under stress, DSTDP molecular chains are attacked accelerated by chemicals; environmental stress cracking is a typical failure mode of polyolefins
Solución
1) Reduce product internal stress, annealing treatment; 2) select high molecular weight DSTDP to improve ESC resistance; 3) avoid contact with aggressive chemicals
Conclusión clave
Stress cracking is caused by stress-accelerated chemical attack; annealing and high MW are key