Extrusion & Post 14 visualizaciones

DSTDP dense surface pockmarks

Fenómeno del problema
DSTDP product surface has dense 0.1-0.3mm pockmarks, affecting appearance and coating adhesion
Análisis de la causa
Raw material contains impurity particles >0.05%; mold cavity surface damage or corrosion pits
Solución
1) Replace with pure raw material, impurities <0.01%; 2) repair and polish mold cavity to Ra<0.2μm; 3) filter raw material to remove particles
Conclusión clave
Pockmarks are caused by raw material impurities and mold damage; pure raw material and mold maintenance are key
DSTDPsurface pockmarksimpurity particlesmold repairpure raw material