Injection Molding 7 visualizaciones

Glass Fibre '2079851475616104452 sink marks

Fenómeno del problema
Glass Fibre injection molded product thick-wall region surface depression 0.2-0.5mm, sink marks
Análisis de la causa
Holding pressure insufficient or holding time short; gate freezes too early, holding pressure cannot be transmitted; wall thickness difference large, after thin wall freezes thick wall cannot be fed
Solución
1) Raise holding pressure 70-90MPa; 2) extend holding to gate freezing +2s; 3) product design reduces wall thickness difference with gradual transition; 4) add supplementary gate in thick-wall region
Conclusión clave
Sink is caused by insufficient holding and wall thickness difference; high-pressure holding and multiple gates are core countermeasures
Glass Fibre injectionsinkholding pressurewall thickness differencegate design