Glass Fibre internal inclusions
Fenómeno del problema
Glass Fibre product interior 0.1-0.5mm inclusions, affecting appearance
Análisis de la causa
Impurity particles in raw material; production environment dust contamination; foreign matter mixed in recycled material
Solución
1) Filter raw material with 120 mesh screen to remove impurities; 2) production environment cleanliness, control dust; 3) strictly sort recycled material to remove foreign matter
Conclusión clave
Inclusions are caused by raw material and environmental contamination; filtration and environment control are key