Molds & Tooling
8 visualizaciones
Glass Fibre product elliptical deformation
Fenómeno del problema
Glass Fibre circular products have ovality >1.03 after demolding
Análisis de la causa
asymmetric demolding force, product deformed by lateral force; uneven cooling, shrinkage differs in all directions
Solución
1) uniform ejection design with 8-point ejection to avoid lateral force; 2) annular uniform cooling; 3) extend cooling time for full setting
Conclusión clave
elliptical deformation is caused by asymmetric demolding force; uniform ejection is key
¿Le ha resultado útil?
0 personas encontraron esto útil