PPSU mold temperature requirements are high

Fenómeno del problema
PPSU needs mold temperature of 140-180°C to obtain optimal performance.
Análisis de la causa
PPSU glass transition temperature is about 220°C; mold temperature needs to be high enough to reduce internal stress and improve performance.
Solución
Use oil temperature unit or electric heating mold to reach and maintain 140-180°C.
Conclusión clave
PPSU's extremely high mold temperature requirement is its processing feature.