Injection Molding 4 visualizaciones

POE '2079851475616104452 flow length ratio insufficient

Fenómeno del problema
POE '2079851475616104452 flow length ratio only 80-100, below 150, thin-walled products cannot be filled
Análisis de la causa
POE melt viscosity high, flow distance short; injection temperature too low; injection pressure insufficient; mold runner resistance large
Solución
1) Raise injection temperature to 160-200°C; 2) Raise injection pressure 80-100MPa; 3) Enlarge runner and gate size to reduce resistance; 4) Add 0.3-0.5wt% flow aid to reduce viscosity
Conclusión clave
Insufficient flow length ratio is caused by high POE viscosity; high temperature, high pressure and large gate are key
POE injectionflow length ratiomelt viscosityinjection temperatureflow aid

¿Le ha resultado útil?

0 personas encontraron esto útil

ChemAI