POE surface microcracks

Fenómeno del problema
POE product surface shows 0.05-0.2mm microcracks, affecting appearance and strength
Análisis de la causa
POE product internal stress too large, exceeding material yield stress; environmental stress cracking; product design stress concentration
Solución
1) Annealing treatment to release internal stress; 2) Product design to avoid sharp corners and stress concentration; 3) Select high molecular weight POE to improve crack resistance
Conclusión clave
Microcracks are caused by excessive internal stress; annealing and crack-resistant design are key
POEmicrocracksinternal stressannealing treatmentstress concentration design