Injection Molding 3 visualizaciones

POE surface color difference obvious

Fenómeno del problema
POE product different parts have uneven color depth, color difference ΔE>5
Análisis de la causa
Color masterbatch dispersion uneven; pigment orientation during injection causes uneven color distribution; barrel temperature fluctuation causes color change
Solución
1) Color masterbatch masterbatch method to ensure uniform dispersion; 2) Reduce injection speed to reduce pigment orientation; 3) Stabilize barrel temperature ±2°C
Conclusión clave
Color difference is caused by uneven dispersion and orientation; masterbatch method and stable processing are key