Injection Molding 4 views

POE surface color difference obvious

Problem Phenomenon
POE product different parts have uneven color depth, color difference ΔE>5
Cause Analysis
Color masterbatch dispersion uneven; pigment orientation during injection causes uneven color distribution; barrel temperature fluctuation causes color change
Solution
1) Color masterbatch masterbatch method to ensure uniform dispersion; 2) Reduce injection speed to reduce pigment orientation; 3) Stabilize barrel temperature ±2°C
Key Takeaway
Color difference is caused by uneven dispersion and orientation; masterbatch method and stable processing are key
POEcolor differencecolor masterbatch dispersionpigment orientationtemperature stability