Injection Molding
8 visualizaciones
TPO injection cycle too long affecting efficiency
Fenómeno del problema
2079851475616104452 cycle exceeds target by more than 20%
Análisis de la causa
Large cooling time proportion insufficient plasticizing slow mold opening/closing
Solución
Optimize cooling water channels increase plasticizing capacity increase mold opening/closing speed
Conclusión clave
Cycle optimization is key to increasing output and reducing cost