Internal shrinkage porosity in PVDF thick-walled products
Fenómeno del problema
The center of thick-walled parts is loose or has voids
Análisis de la causa
The center cools slowly and the feeding channel solidifies prematurely
Solución
Optimize the gate position and size, extend holding pressure, and increase pressure
Conclusión clave
The internal quality of thick-walled parts is a technical difficulty