Rubber Migration/Bleeding of Cast Polypropylene Film HIPS Products
Fenómeno del problema
Rubber migration or bleeding appears on the surface of HIPS products, and the surface becomes sticky or discolored, affecting the product appearance and printing performance.
Análisis de la causa
(1) The rubber content is too high or the compatibility with the base material is poor
(2) The processing temperature is too high, and the rubber partially degrades and migrates
(3) The storage temperature of the product is high, accelerating rubber migration
(4) The rubber particle size is too large, making it easy to migrate
(5) Additives interact with the rubber and promote migration
Solución
(1) Select a grade with suitable rubber content and compatibility
(2) Control the processing temperature within the range of 230-270°C
(3) The storage temperature of the product does not exceed 40°C
(4) Select a grade with a small rubber particle size
(5) Reduce additives that may interact with the rubber
Conclusión clave
HIPS rubber bleeding is caused by compatibility and temperature.