Extrusion & Post
8 visualizaciones
Poor printability of metallocene linear low-density polyethylene film (variant: strengthened measures)
Fenómeno del problema
Printing ink adhesion on the film surface is poor, and printed patterns fall off or are blurred.
Poor printability affects product appearance and affects product quality in printed packaging film.
Especially, additional attention is needed on top of the original basis; this problem is more prominent and requires focused attention.
Análisis de la causa
(1) Metallocene linear low-density polyethylene has low surface energy (<32dyn/cm), and ink wettability is poor
(2) Film surface treatment is insufficient (corona treatment is not enough)
(3) There are exudates on the film surface (migration of slip agents and antiblocking agents)
(4) The ink does not match the film
(5) Printing environment humidity is improper
(6) On top of the original basis, additional attention is needed as process parameter fluctuations or equipment condition changes aggravate this problem
Solución
(1) Perform corona treatment to increase film surface tension to 38-42dyn/cm
(2) Control corona treatment power and treatment time to ensure uniform treatment
(3) Control additive dosage to avoid excessive migration
(4) Select ink types that match the film
(5) Control printing environment humidity at 50-60%
(6) And strengthen process monitoring; on top of the original basis, additional attention is needed to pay special attention to parameter stability
Conclusión clave
Poor printability is caused by low surface energy and needs to be improved by increasing surface tension through corona treatment to improve ink adhesion.
In different production scenarios, targeted preventive measures need to be taken.
¿Le ha resultado útil?
0 personas encontraron esto útil
¡Gracias por sus comentarios!