Uneven wall thickness of cross-linked polyethylene extruded pipes (Variant: mass production scenario)
Fenómeno del problema
The wall thickness of the pipe is uneven in the circumferential direction, showing eccentric wall phenomenon.
Uneven wall thickness affects the pressure resistance of the pipe; the thin-walled side ruptures first under pressure, seriously affecting the safety of pipe use.
Especially in continuous mass production, this problem is more prominent and requires key attention.
Análisis de la causa
(1) Die and mandrel not concentric, gap uneven
(2) Melt temperature uneven, large circumferential temperature difference at the die
(3) Extruder output uneven, melt pressure fluctuates
(4) Haul-off speed unstable or haul-off center not concentric with the die
(5) Pipe sizing sleeve worn or improperly installed
(6) In continuous mass production, process parameter fluctuations or equipment state changes aggravate this problem
Solución
(1) Adjust the concentricity of die and mandrel, circumferential gap error not exceeding ±0.05mm
(2) Check die heating ring distribution, ensure circumferential temperature difference not exceeding ±3°C (170-220°C range)
(3) Check extruder plasticizing stability to ensure uniform output
(4) Adjust the center line of the haul-off device to align with the die center
(5) Check the sizing sleeve, replace if severely worn, ensure concentric installation
(6) And establish standardized work instructions, paying special attention to parameter stability in continuous mass production
Conclusión clave
Uneven wall thickness is caused by uneven die gap or uneven temperature, and needs to be solved from mold accuracy and temperature uniformity.
Targeted preventive measures need to be taken in different production scenarios.