Glass fiber exposure of PBT reinforced materials

Fenómeno del problema
The glass fiber on the surface of glass fiber reinforced PBT products is obviously exposed, with a rough feel.
Análisis de la causa
The mold temperature is too low, and the surface layer PBT cools quickly and cannot fully coat the glass fiber; the injection speed is too slow; the glass fiber content is too high or the length is too long.
Solución
Raise the mold temperature to 100-120°C; increase the injection speed to achieve fast mold filling; appropriately reduce the glass fiber content or use chopped glass fiber.
Conclusión clave
PBT glass fiber exposure is closely related to mold temperature and mold filling speed.