Material Drying
7 visualizaciones
Gel particles and fisheyes on PET sheet surface
Fenómeno del problema
Transparent or opaque tiny particles appear on the PET extruded sheet surface, affecting appearance and subsequent processing.
Análisis de la causa
Material mixed with high-melting impurities or crosslinked gels, material stays too long at screw dead corners forming gels, drying temperature too high causing solid-state polycondensation.
Solución
Clean screw and barrel to eliminate dead corners; control drying temperature ≤175°C; appropriately increase processing temperature to melt gel particles; use filter screens.
Conclusión clave
PET gel particles originate from impurities, degradation, or excessive drying.