Gel particles and fisheyes on PET sheet surface
Fenómeno do problema
Transparent or opaque tiny particles appear on the PET extruded sheet surface, affecting appearance and subsequent processing.
Análise das causas
Material mixed with high-melting impurities or crosslinked gels, material stays too long at screw dead corners forming gels, drying temperature too high causing solid-state polycondensation.
Solução
Clean screw and barrel to eliminate dead corners; control drying temperature ≤175°C; appropriately increase processing temperature to melt gel particles; use filter screens.
Conclusão principal
PET gel particles originate from impurities, degradation, or excessive drying.