Molding Process 6 visualizaciones

Poor adhesion of PET vacuum aluminized film

Fenómeno del problema
After vacuum aluminizing of PET film, the aluminum layer has poor adhesion and easily falls off or scratches.
Análisis de la causa
Low surface energy of PET film (about 30-36mN/m), surface contamination (oil, dust), improper aluminizing process parameters.
Solución
Corona treat PET film to dyne value ≥42mN/m; ensure film surface cleanliness; optimize aluminizing parameters vacuum ≤5×10⁻⁴Pa.
Conclusión clave
PET aluminized film adhesion depends on surface treatment and coating process.
PETaluminizingadhesioncorona treatmentsurface energy