Extrusion & Post 6 visualizaciones

Poor transparency and haze in PET film

Fenómeno del problema
PET biaxially stretched film has poor transparency and a high haze value.
Análisis de la causa
The content of additives (slip agents, antiblocking agents) in the raw material is too high or particle size is too large; improper stretching temperature causes incomplete crystallization.
Solución
Select low-haze grade PET raw material; optimize stretching temperature (longitudinal 90-110°C, transverse 100-120°C); control cooling rate.
Conclusión clave
PET film transparency is influenced by both raw material formulation and the stretching process.
PETfilmhazebiaxial stretchingadditives