Thermoforming 8 visualizaciones

Low interlayer peel strength of PET composite sheet

Fenómeno del problema
PET/PE or PET/EVOH composite sheets delaminate during '2079851475616104458 or use.
Análisis de la causa
Adhesive layer thickness is insufficient or improperly selected; melt temperatures of each layer do not match; lamination pressure is insufficient; shrinkage differences between layers are large.
Solución
Optimize adhesive layer material and thickness; adjust the temperature of each layer to match viscosities; increase laminating roller pressure.
Conclusión clave
The interlayer bonding force of PET composite sheet depends on the adhesive layer and the process matching of each layer.
PETcomposite sheetdelaminationadhesive layertemperature matching