Menú
Materiales Maquinaria
Perspectivas
Artículos Vídeos Problema y solución
About
Acerca de Chembull Socios de medios
Contáctenos
Idioma
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
Volver a Problema y solución
Extrusion & Post 7 visualizaciones

High boiling water shrinkage rate of PET fiber

Fenómeno del problema
The boiling water shrinkage rate of PET fiber exceeds the standard (>5%), and the dimensions of finished products are unstable.
Análisis de la causa
Insufficient heat setting after fiber drawing results in high molecular chain internal stress; draw ratio is too large; heat setting temperature is low or time is short.
Solución
Increase heat setting temperature and extend setting time; appropriately reduce the draw ratio; adopt relaxation heat treatment process.
Conclusión clave
PET fiber boiling water shrinkage rate reflects the internal stress level; full heat setting is the control means.
PETfiberboiling water shrinkageheat settinginternal stress

¿Le ha resultado útil?

0 personas encontraron esto útil

ChemAI