Extrusion & Post
7 visualizaciones
PLA barrier coating technology
Fenómeno del problema
Process problems of adhesion when coating PLA film with high barrier coating.
Análisis de la causa
The interface bonding force between the coating and the PLA film is temperature sensitive.
Solución
Pre-corona treat the film surface; optimize the coating curing and drying temperature.
Conclusión clave
PLA barrier coating requires film pretreatment.
¿Le ha resultado útil?
0 personas encontraron esto útil